Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cardia Compostable B-F12 - (PSAC+Polyester) - Cardia Bioplastics

Material Data Center offers the following functions for Cardia Compostable B-F12:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cardia Compostable datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 2.55 g/10min ASTM D 1238
温度 190 °C -
负载 2.61 kg -
热性能价值单位Test Standard
ASTM数据
熔点 94 °C ASTM D 3418
其它性能价值单位Test Standard
密度 1200 kg/m³ ASTM D 792
Moisture Content 0.6 % -
机械性能(薄膜)价值单位Test Standard
ASTM Data
拉伸模量, 平行 220 MPa ASTM D 882
拉伸模量, 垂直 140 MPa ASTM D 882
拉伸强度, 平行 28 MPa ASTM D 882
拉伸强度, 垂直 22 MPa ASTM D 882
断裂伸长率, 平行 270 % ASTM D 882
断裂伸长率, 垂直 470 % ASTM D 882
挤出形式 麓碌陇 - -
试样厚度 0.02 mm -
加工推荐(挤出)价值单位Test Standard
Type of extrusion blown - -
加料温度 120 - 150 °C -
1区 130 - 160 °C -
2区 140 - 165 °C -
3区 140 - 165 °C -
喷嘴温度 135 - 165 °C -
典型数据
加工方法
吹塑挤出成型, 薄膜挤出成型
供货形式
黑色, 棕色, 自然色
添加剂
增塑剂
Certifications
生物相容, 生物降解, 可食品接触的, 可堆肥 ISO 13432 (制造商), 可堆肥 ASTM D6400 (制造商), 可堆肥 ISO 13432 (证书), 可堆肥 ASTM D6400 (证书)
应用
包装
地区供应
北美, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.